Salts for electrolytic degreasing. It strongly degreases any metallic surface, leaving it ready to apply any galvanic bath or subsequent patina. It is an essential process before applying any type of bath or chemical treatment.
Characteristics: Voltage: from 4 to 6 V stainless steel anode Working time: between 30 and 60 seconds Can be used with any metal Working temperature: ambient Preparation: Mix 50 grams per liter of distilled water, reserving half a liter of the total you want to prepare. Shake vigorously until you notice an increase in temperature in the preparation. Introduce into the working tank and add another half liter of distilled water.